Medtronic Recalls HVAD Pump Implant Kit for Pump Weld Defect
Murilo Freitas - 04:00, 9 de junio de 2022554
0
Medtronic recalls pump implant kit due to a pump weld defect that may lead to corrosion of pump internal parts and cause the pump to rotate incorrectly.